Steel Melting Point: A Proven, Complete Grade-by-Grade Chart

Reading Time: 7 minutes
Infographic titled “Steel Melting Point: Grade-by-Grade Chart” from C.L. Dews & Sons, featuring an image of molten metal in a foundry furnace.

Foundry Metallurgy

Steel Melting Point and Iron Melting Ranges: The Complete Grade-by-Grade Chart

Toss a clean steel offcut into a furnace of molten gray iron held at 2,550°F and it still vanishes. That surprises people, because the steel melting point sits a couple of hundred degrees higher, somewhere around 2,600 to 2,800°F. The iron never gets hot enough to melt the steel. Instead, carbon from the bath soaks into the steel’s surface, drags the melting temperature of that thin skin down below the bath temperature, and the offcut dissolves layer by layer like sugar in hot coffee.

That one bit of furnace behavior sums up what matters about melting ferrous metals. There is no single number for “steel” or “iron,” the range moves with chemistry, and carbon is the biggest lever of all. Here is the reference chart we work from when people ask.

Key Takeaways
  • Pure iron melts at 2,800°F (1,538°C). Every alloy addition, carbon above all, pulls that number down.
  • Carbon steel melts across roughly 2,600 to 2,800°F (1,425 to 1,540°C). Common stainless grades run about 2,500 to 2,790°F (1,375 to 1,530°C).
  • Gray cast iron melts several hundred degrees lower, around 2,060 to 2,200°F (1,127 to 1,204°C), which is a big reason iron is so castable.
  • Alloys melt between a solidus and a liquidus, not at one temperature. The width of that gap decides how a casting shrinks and how it must be fed.
  • Foundries pour well above the liquidus. Steel castings typically pour hundreds of degrees hotter than iron, which raises cost and difficulty at every step.

Steel Melting Point at a Glance

The short answer: most carbon and low-alloy steels are fully liquid somewhere between 2,600 and 2,800°F (about 1,425 to 1,540°C). The exact figure for a given steel depends mainly on its carbon content. A low-carbon structural steel melts close to pure iron, while a high-carbon tool steel starts melting noticeably lower.

Pure iron is the ceiling for this whole family. The Royal Society of Chemistry’s iron data lists its melting point at 1,538°C, or 2,800°F. Everything else on the chart is iron with something added, and almost every addition lowers the temperature at which melting begins.

Steel Melting Point Chart by Grade

The ranges below are the commonly published values for each material. Treat them as reference figures, not a spec. Any specific heat shifts with its exact chemistry, so the mill test report or the alloy’s data sheet beats a general chart every time.

MaterialMelting Range (°F)Melting Range (°C)Notes
Pure iron2,8001,538Single melting point; the reference ceiling
Wrought iron2,700 to 2,9001,482 to 1,593Nearly pure iron with strings of glassy slag
Carbon steel2,600 to 2,8001,425 to 1,540Lower end for higher carbon grades
410 stainless2,700 to 2,7901,480 to 1,530Martensitic, about 12% chromium
430 stainless2,600 to 2,7501,425 to 1,510Ferritic, about 17% chromium
304 stainless2,550 to 2,6501,400 to 1,450Austenitic, 18% chromium, 8% nickel
316 stainless2,500 to 2,5501,375 to 1,400Austenitic with molybdenum added
Gray cast iron2,060 to 2,2001,127 to 1,204Roughly 2.5 to 4% carbon, near the eutectic
Ductile ironAbout 2,100About 1,150Similar carbon to gray iron, graphite as spheres

Put them on one temperature scale and the pattern is hard to miss: the steels and wrought iron crowd into a tight band just under pure iron, and the cast irons sit far to the left.

Melting ranges of iron and steel grades on a 2,000 to 3,000 degree F scale: gray cast iron 2,060 to 2,200 F, 316 stainless 2,500 to 2,550 F, 304 stainless 2,550 to 2,650 F, carbon steel 2,600 to 2,800 F, 430 stainless 2,600 to 2,750 F, 410 stainless 2,700 to 2,790 F, wrought iron 2,700 to 2,900 F, pure iron 2,800 F Gray cast iron 316 stainless 304 stainless Carbon steel 430 stainless 410 stainless Wrought iron Pure iron 2,060 to 2,200 F 2,500 to 2,550 F 2,550 to 2,650 F 2,600 to 2,800 F 2,600 to 2,750 F 2,700 to 2,790 F 2,700 to 2,900 F 2,800 F (1,538 C) 2,000 2,200 2,400 2,600 2,800 3,000 Temperature (degrees F)
Commonly published melting ranges for iron and steel grades. The dashed line marks pure iron at 2,800°F (1,538°C).

1. Carbon Steel

Carbon steel covers the widest everyday range because its carbon content varies so much. A mild steel near 0.1% carbon finishes melting close to 2,780°F, while a 1% carbon steel starts melting well under 2,600°F. Manganese, silicon, and other small additions nudge the numbers further.

2. Stainless Steel

Chromium alone does not drop the melting range much, which is why ferritic and martensitic grades like 430 and 410 sit close to carbon steel. Nickel and molybdenum pull it lower, so the austenitic workhorses, 304 and 316, are the lowest-melting stainless grades on the chart.

3. Cast Iron

Cast iron carries more than ten times the carbon of a typical structural steel, and that carbon is why it melts several hundred degrees lower. At about 4.3% carbon, iron and carbon form a eutectic that freezes at a single temperature of roughly 2,100°F (1,148°C). Most gray and ductile irons are deliberately designed to sit near that point.

4. Wrought Iron

Wrought iron is almost carbon-free iron threaded with fibers of glassy slag. The iron itself melts close to pure iron, which is why the published range runs so high, while the slag softens far lower. Very little true wrought iron is made today, and most “wrought iron” railings are actually mild steel.

Why Alloys Melt Over a Range, Not at One Temperature

A pure metal melts the way an ice cube does: at one temperature, all at once. An alloy behaves more like slush. As it heats, it reaches a solidus, where the first liquid appears between the grains. It keeps absorbing heat through a mushy zone of mixed solid and liquid until it reaches the liquidus, where the last solid disappears.

Why? Different elements favor the liquid or the solid to different degrees. As the alloy freezes, the first crystals that form are purer iron, pushing carbon and other elements into the remaining liquid. That enriched liquid now has a lower freezing point, so it holds out longer. The result is a temperature window instead of a single steel melting point.

Shop-floor shortcut: when a chart gives a range, the low number is roughly where melting starts (solidus) and the high number is where the metal is fully liquid (liquidus). Pouring always happens above the high number.

The eutectic is the exception. A gray iron right at the eutectic composition freezes almost like a pure metal, with a very narrow window, and that single property shapes a huge share of foundry practice.

How the Steel Melting Point Drives Foundry Practice

In our metal casting foundry, melting temperature is not trivia. It sets the furnace schedule, the ladle practice, the mold design, and a good part of the cost of every casting.

1. Superheat and Pouring Temperature

Metal has to leave the ladle well above its liquidus. That extra heat, called superheat, keeps it fluid while it travels through the gating and fills thin sections before freezing. Gray iron commonly pours somewhere around 2,450 to 2,700°F depending on section size, a few hundred degrees above its liquidus. Carbon and low-alloy steel castings typically pour around 2,850 to 3,100°F because their liquidus starts so much higher.

Foundry worker dipping an immersion thermocouple lance into a ladle of molten gray iron to confirm pouring temperature

So every ladle gets a temperature check right before it pours. A long immersion thermocouple goes into the metal, and if the reading has drifted below the target window, that ladle does not go on a thin-walled mold. Pour too cold and you get misruns and cold shuts. Pour too hot and you invite gas pickup, mold erosion, and rough surfaces.

2. Freezing Range Decides How a Casting Is Fed

Most metals shrink as they freeze, so foundries add risers, reservoirs of liquid metal that feed the casting as it contracts. Gray iron near the eutectic is the lucky exception. As it freezes, graphite precipitates and expands, offsetting much of the shrinkage, so well-designed gray iron castings often need surprisingly little feeding.

Steel gets no such help. It shrinks substantially on freezing and needs large risers, sometimes adding a big share of extra metal to the pour weight. High-chrome white irons, like the 15, 25, and 28% chrome grades we pour for crusher wear parts, form hard carbides instead of graphite, so they also shrink more and need careful feeding. Our comparison of high chrome vs manganese steel for crusher wear parts covers why those alloys are still worth the extra work.

3. Hotter Metal Is Harder on Everything

Every hundred degrees costs something. Higher temperatures wear furnace and ladle linings faster, burn more energy, and attack mold sand harder. Liquid steel also dissolves more hydrogen and other gases than liquid iron does, so steel melting demands tighter control of charge materials and moisture. That is part of why iron castings are usually the lower-cost route when the part’s strength requirements allow it.

4. Steel Scrap as a Charge Material

This is the vanishing offcut put to work. Iron foundries routinely add clean steel scrap to the charge to dilute carbon and control chemistry. The scrap dissolves the same way the offcut did: carbon from the bath diffuses in and lowers its surface melting temperature, even though the bath never reaches the steel’s own melting range. That takes time, which is why scrap size and charging order matter.

What Melting Temperature Means in Fabrication and Welding

Outside the foundry, melting temperature shows up in quieter ways. In steel fabrication, a weld pool has to be fully liquid at the fusion line, so the arc pushes the base metal briefly past its liquidus while the surrounding steel stays solid. Oxy-fuel cutting is different: the torch heats steel to its ignition temperature, well below melting, and the oxygen jet burns a path through it.

The more important number for structures is not the melting point at all. Steel loses a large share of its strength long before it melts, which is why fire protection on building steel is designed around far lower temperatures than anything on the chart above.

Frequently Asked Questions

Does stainless steel melt at a lower temperature than carbon steel?

Usually, yes, but not by much. Austenitic grades like 304 and 316 melt roughly 100 to 250°F lower than typical carbon steel because of their nickel and molybdenum. Ferritic and martensitic grades land close to carbon steel.

Why does cast iron melt so much lower than steel?

Carbon. Raising carbon from a fraction of a percent to around 3 or 4% drops the melting range by roughly 600°F, which makes cast iron easier to melt and much more fluid when poured.

Is the steel melting point the same as the pouring temperature?

No. Pouring temperature is always above the liquidus, often by a few hundred degrees for iron and by less for steel, so the metal stays fluid long enough to fill the mold.

Talk Metallurgy With a Foundry That Pours Every Day

Melting ranges look simple on a chart. Turning them into sound castings takes the right alloy, the right pouring window, and a feeding plan matched to how that metal freezes. Our crew in Hattiesburg, Mississippi melts, pours, heat treats, and machines under one roof, from gray iron castings to high-chrome wear parts.

Send us a drawing or a worn part, and we will tell you which alloy we would pour and how we would make it.

Request a Quote

Call 601-582-4427

SHARE:

Request a Quote

Iframe code